Rotate the inserted parts clockwise, and no convex phenomenon appears;
The inserted parts can be changed from the front face, and when rotating it 2-4 circles anticlockwise, convex phenomenon appears, and it is easy to replace without removing the mould;
Note: in the production process, don't rotate anticlockwise when adjusting the date stamp, and you should adjust it clockwise to avoid then inserted parts loose.
Part No | FX.0632SF; FX.0847SF.... |
Material | SUS420 |
Hardness | 48-54 |
Inner Pointer of date stamp:
Inner pointer can be dismantled, and you can choose different types of inner pointer according to different years.